Studies on initial stage of high temperature oxidation of Fe - 9 to 12% Cr alloys in water vapour environment
Fe - 9 to 12%Cr alloys are a material for the thick sections boiler components and steam lines of a power plant. The role Fe - 9 to 12%Cr alloys is becoming more prominent in the development of a new generation of Ultra-Supercritical (USC) Power Plant due to the target operating temperature is re...
Main Authors: | Kaderi, Akbar, Ani, Mohd Hanafi, Herman, Sukreen Hana, Othman, Raihan |
---|---|
Format: | Article |
Language: | English |
Published: |
Trans Tech Publications, Switzerland
2012
|
Subjects: | |
Online Access: | http://irep.iium.edu.my/27470/ http://irep.iium.edu.my/27470/ http://irep.iium.edu.my/27470/1/Studies_on_initial_stage_of_high_temperature_oxidation_of_fe-9_to_12cr_alloys_in_water_vapour_environment.pdf |
Similar Items
-
Observation on void formed in oxide scale of Fe-Cr-Ni alloy at 1073K in dry and humid environments
by: Kaderi, Akbar, et al.
Published: (2011) -
Internal oxidation of Ni-Cr-Al alloys under various oxygen partial pressures at 1273 K
by: Ani, Mohd Hanafi, et al.
Published: (2012) -
Initial stage oxidation of cr in dry and wet environment at 1073 K and the significant differences of FT – IR spectra produced thereof
by: Kaderi, Akbar, et al.
Published: (2012) -
Microstructural evaluation and corrosion behaviour of Fe-Cr-Ni-Mn-Co AND AI0.5-Fe-Cr-Ni-Mn-Co highentropy alloys (HEA) with elemental additions / Siti Sarah Mohd Pauzi
by: Mohd Pauzi, Siti Sarah
Published: (2018) -
Formation of protective Cr2O3 scale at high temperature and the effect of mass transport in the presence of water vapor
by: Ani, Mohd Hanafi, et al.
Published: (2012)