The effect of peroxyacetic acid treatment at elevated temperature onto the Indonesian coal microstructure
A sub-bituminous high sulphur Indonesian coal, namely Banjarmasin Hj. Ali-Aliansar (BMHA) has been treated with peroxyacetic acid, a mild oxidising agent at temperature of 70°C and at atmospheric pressure. Initial findings have shown that this reagent is capable of removing up to 60 % of the total s...
Main Authors: | Mohd Ishak, Mohd Azlan, Ismail, Khudzir, Ismail, Ahmad Faris |
---|---|
Format: | Article |
Language: | English |
Published: |
Faculty of Applied Science, Universiti Teknologi MARA
2004
|
Subjects: | |
Online Access: | http://irep.iium.edu.my/36838/ http://irep.iium.edu.my/36838/1/Science_Letters.pdf |
Similar Items
-
The effect of peroxyacetic acid treatment at elevated temperature onto the Indonesian coal microstructure / Mohd Azlan Mohd Ishak, Khudzir Ismail and Ahmad Faris Ismail
by: Mohd Ishak, Mohd Azlan, et al.
Published: (2004) -
The influence of temperature on adsorption capacity of Malaysian coal
by: Azmi, Azlin Suhaida, et al.
Published: (2006) -
Ductile-brittle transition temperature of polylactic acid-based biocomposite
by: Kaiser, Mohammad Rejaul, et al.
Published: (2013) -
Optimization of manganese reduction in biotreated POME onto 3A molecular sieve and clinoptilolite zeolites
by: Jami, Mohammed Saedi, et al.
Published: (2016) -
Extraction of glucose from kenaf core using mild acid treatment
by: Seeni Mohamed, Nurhafizah, et al.
Published: (2012)