In vitro recellularization of aorta scaffolds prepared by sonication treatment
Sonication treatment is used in the preparation of bioscaffolds that was able to support repopulation of vascular smooth muscle cells (VSMCs) upon cell-seeding. The aim of this study is to investigate the ability of sonicatedly decellularized tissue to repopulate VSMCs after 6 days of cell-seeding....
Main Authors: | , , |
---|---|
Format: | Conference or Workshop Item |
Language: | English English |
Published: |
2015
|
Subjects: | |
Online Access: | http://irep.iium.edu.my/44926/ http://irep.iium.edu.my/44926/ http://irep.iium.edu.my/44926/ http://irep.iium.edu.my/44926/1/In_vitro_recellularization_of_aorta_scaffolds_prepared_by_sonication_treatment.pdf http://irep.iium.edu.my/44926/4/ascc_proceeeding_cove%2C_copyright%2C_content.pdf |
id |
iium-44926 |
---|---|
recordtype |
eprints |
spelling |
iium-449262016-05-23T05:36:31Z http://irep.iium.edu.my/44926/ In vitro recellularization of aorta scaffolds prepared by sonication treatment Syazwani, N. Ushida, T. Azhim, Azran TP248.13 Biotechnology Sonication treatment is used in the preparation of bioscaffolds that was able to support repopulation of vascular smooth muscle cells (VSMCs) upon cell-seeding. The aim of this study is to investigate the ability of sonicatedly decellularized tissue to repopulate VSMCs after 6 days of cell-seeding. In this study, sample of aorta tissues are decellularized by sonication treatment in 0.1% and 2% sodium dodecyl sulfate (SDS) detergent for 10 hours. It was followed by washing process with PBS solution for 5 days. Decellularized aorta tissues are then cell seeded with VSMCs by static seeding in 96-well plate containing Dulbecco's Modified Eagle Medium (DMEM) at 37°C. The infiltrations of VSMCs onto decellularized tissues are evaluated by comparison of Hematoxylin-Eosin (H-E) staining at 0 and 6 days of cell-seeding. The histological results of cell-seeding showed that VSMCs are able to infiltrate onto the decellularized tissues. From the results, sonicatedly decellularized tissue treated in 0.1% and 2% SDS, seeded with VSMCs showed infiltration depth of 0.43 mm and 0.35 mm, respectively. Hence, a sonicated decellularized tissue treated with 0.1% and 2% SDS was shown to support the repopulation of VSMCs. 2015 Conference or Workshop Item PeerReviewed application/pdf en http://irep.iium.edu.my/44926/1/In_vitro_recellularization_of_aorta_scaffolds_prepared_by_sonication_treatment.pdf application/pdf en http://irep.iium.edu.my/44926/4/ascc_proceeeding_cove%2C_copyright%2C_content.pdf Syazwani, N. and Ushida, T. and Azhim, Azran (2015) In vitro recellularization of aorta scaffolds prepared by sonication treatment. In: The 10th Asian Control Conference (ASCC 2015), 31 May - 3 June 2015, Kota Kinabalu, Sabah. http://dx.doi.org/10.1109/ASCC.2015.7244769 doi:10.1109/ASCC.2015.7244769 |
repository_type |
Digital Repository |
institution_category |
Local University |
institution |
International Islamic University Malaysia |
building |
IIUM Repository |
collection |
Online Access |
language |
English English |
topic |
TP248.13 Biotechnology |
spellingShingle |
TP248.13 Biotechnology Syazwani, N. Ushida, T. Azhim, Azran In vitro recellularization of aorta scaffolds prepared by sonication treatment |
description |
Sonication treatment is used in the preparation of bioscaffolds that was able to support repopulation of vascular smooth muscle cells (VSMCs) upon cell-seeding. The aim of this study is to investigate the ability of sonicatedly decellularized tissue to repopulate VSMCs after 6 days of cell-seeding. In this study, sample of aorta tissues are decellularized by sonication treatment in 0.1% and 2% sodium dodecyl sulfate (SDS) detergent for 10 hours. It was followed by washing process with PBS solution for 5 days. Decellularized aorta tissues are then cell seeded with VSMCs by static seeding in 96-well plate containing Dulbecco's Modified Eagle Medium (DMEM) at 37°C. The infiltrations of VSMCs onto decellularized tissues are evaluated by comparison of Hematoxylin-Eosin (H-E) staining at 0 and 6 days of cell-seeding. The histological results of cell-seeding showed that VSMCs are able to infiltrate onto the decellularized tissues. From the results, sonicatedly decellularized tissue treated in 0.1% and 2% SDS, seeded with VSMCs showed infiltration depth of 0.43 mm and 0.35 mm, respectively. Hence, a sonicated decellularized tissue treated with 0.1% and 2% SDS was shown to support the repopulation of VSMCs. |
format |
Conference or Workshop Item |
author |
Syazwani, N. Ushida, T. Azhim, Azran |
author_facet |
Syazwani, N. Ushida, T. Azhim, Azran |
author_sort |
Syazwani, N. |
title |
In vitro recellularization of aorta scaffolds prepared by sonication treatment |
title_short |
In vitro recellularization of aorta scaffolds prepared by sonication treatment |
title_full |
In vitro recellularization of aorta scaffolds prepared by sonication treatment |
title_fullStr |
In vitro recellularization of aorta scaffolds prepared by sonication treatment |
title_full_unstemmed |
In vitro recellularization of aorta scaffolds prepared by sonication treatment |
title_sort |
in vitro recellularization of aorta scaffolds prepared by sonication treatment |
publishDate |
2015 |
url |
http://irep.iium.edu.my/44926/ http://irep.iium.edu.my/44926/ http://irep.iium.edu.my/44926/ http://irep.iium.edu.my/44926/1/In_vitro_recellularization_of_aorta_scaffolds_prepared_by_sonication_treatment.pdf http://irep.iium.edu.my/44926/4/ascc_proceeeding_cove%2C_copyright%2C_content.pdf |
first_indexed |
2023-09-18T21:03:53Z |
last_indexed |
2023-09-18T21:03:53Z |
_version_ |
1777410804148076544 |