Cotton wastes for composite reinforcement / Mohd Iqbal Misnon

This study assesses the possibility of fabricating composites out of cotton waste. Two (2) types of cotton wastes were taken from a spinning mill and used in this study , which were blowing waste and comb noils. Two (2) types of matrices were used in this project: polyester resin (thermosets) and...

Full description

Bibliographic Details
Main Author: Misnon, Mohd Iqbal
Format: Thesis
Language:English
Published: 2007
Subjects:
Online Access:http://ir.uitm.edu.my/id/eprint/27358/
http://ir.uitm.edu.my/id/eprint/27358/1/TM_MOHD%20IQBAL%20MISNON%20AS%2007_5.pdf
id uitm-27358
recordtype eprints
spelling uitm-273582020-01-21T03:40:31Z http://ir.uitm.edu.my/id/eprint/27358/ Cotton wastes for composite reinforcement / Mohd Iqbal Misnon Misnon, Mohd Iqbal Weights and measures Cotton manufactures This study assesses the possibility of fabricating composites out of cotton waste. Two (2) types of cotton wastes were taken from a spinning mill and used in this study , which were blowing waste and comb noils. Two (2) types of matrices were used in this project: polyester resin (thermosets) and polypropylene (thermoplastic). Composite materials were fabricated using compression with mould (hot press) for thermoplastic resin and compression without mould for thermoset resin. Tensile and flexural test were done in order to assess the mechanical properties of cotton waste composites. Statistical analysis using ANOVA (analysis of variance) and post hoc; Duncan were derived to test any significant difference in tensile and flexural strength results. Comb noils-polyester composite was found to produce the highest result in tensile and flexural strength which are 71.01 MPa and 126.85 MPa respectively. The lowest is exhibited by blowing waste-polyester composite which is 48.73 MPa and 83.63 MPa for tensile and flexural strength. Comb noils-polypropylene composite also show the highest tensile and flexural strength of 54.22 MPa and 75.60 MPa respectively and the lowest is exhibited by comb noils-polypropylene composite via crushing method which are 26.97 MPa for tensile and 58.75 MPa for flexural strength. Regression and correlation analysis was also done in order to determine the trend of all the parameters. Good relationship between tensile and flexural properties was also found with cotton waste composites. It was also found that a positive correlation existed for tensile and flexural prop~rties with the length of the waste fibres used . The longer the length of the fibres , the higher would be the strength. However , this is only true for normal size textile fibres and not the nano and other smaller size fibres. 2007 Thesis NonPeerReviewed text en http://ir.uitm.edu.my/id/eprint/27358/1/TM_MOHD%20IQBAL%20MISNON%20AS%2007_5.pdf Misnon, Mohd Iqbal (2007) Cotton wastes for composite reinforcement / Mohd Iqbal Misnon. Masters thesis, Universiti Teknologi MARA.
repository_type Digital Repository
institution_category Local University
institution Universiti Teknologi MARA
building UiTM Institutional Repository
collection Online Access
language English
topic Weights and measures
Cotton manufactures
spellingShingle Weights and measures
Cotton manufactures
Misnon, Mohd Iqbal
Cotton wastes for composite reinforcement / Mohd Iqbal Misnon
description This study assesses the possibility of fabricating composites out of cotton waste. Two (2) types of cotton wastes were taken from a spinning mill and used in this study , which were blowing waste and comb noils. Two (2) types of matrices were used in this project: polyester resin (thermosets) and polypropylene (thermoplastic). Composite materials were fabricated using compression with mould (hot press) for thermoplastic resin and compression without mould for thermoset resin. Tensile and flexural test were done in order to assess the mechanical properties of cotton waste composites. Statistical analysis using ANOVA (analysis of variance) and post hoc; Duncan were derived to test any significant difference in tensile and flexural strength results. Comb noils-polyester composite was found to produce the highest result in tensile and flexural strength which are 71.01 MPa and 126.85 MPa respectively. The lowest is exhibited by blowing waste-polyester composite which is 48.73 MPa and 83.63 MPa for tensile and flexural strength. Comb noils-polypropylene composite also show the highest tensile and flexural strength of 54.22 MPa and 75.60 MPa respectively and the lowest is exhibited by comb noils-polypropylene composite via crushing method which are 26.97 MPa for tensile and 58.75 MPa for flexural strength. Regression and correlation analysis was also done in order to determine the trend of all the parameters. Good relationship between tensile and flexural properties was also found with cotton waste composites. It was also found that a positive correlation existed for tensile and flexural prop~rties with the length of the waste fibres used . The longer the length of the fibres , the higher would be the strength. However , this is only true for normal size textile fibres and not the nano and other smaller size fibres.
format Thesis
author Misnon, Mohd Iqbal
author_facet Misnon, Mohd Iqbal
author_sort Misnon, Mohd Iqbal
title Cotton wastes for composite reinforcement / Mohd Iqbal Misnon
title_short Cotton wastes for composite reinforcement / Mohd Iqbal Misnon
title_full Cotton wastes for composite reinforcement / Mohd Iqbal Misnon
title_fullStr Cotton wastes for composite reinforcement / Mohd Iqbal Misnon
title_full_unstemmed Cotton wastes for composite reinforcement / Mohd Iqbal Misnon
title_sort cotton wastes for composite reinforcement / mohd iqbal misnon
publishDate 2007
url http://ir.uitm.edu.my/id/eprint/27358/
http://ir.uitm.edu.my/id/eprint/27358/1/TM_MOHD%20IQBAL%20MISNON%20AS%2007_5.pdf
first_indexed 2023-09-18T23:18:19Z
last_indexed 2023-09-18T23:18:19Z
_version_ 1777419261652762624