Effect of space holders on fabrication of porous titanium alloy-hydroxyapatite composite through powder injection molding

Powder injection molding (PIM) is able to produce porous titanium alloy/hydroxyapatite composite through the space holder technique. Thermal debinding and sintering processes were the main challenges due to different properties of metal and ceramic in producing such composite. This study focused on...

Full description

Bibliographic Details
Main Authors: Farrahshaida Mohd Salleh, Abu Bakar Sulong, Muhammad Rafi Raza, Norhamidi Muhamad, Lim, Tsiu Fhang
Format: Article
Language:English
Published: Penerbit Universiti Kebangsaan Malaysia 2017
Online Access:http://journalarticle.ukm.my/11395/
http://journalarticle.ukm.my/11395/
http://journalarticle.ukm.my/11395/1/38%20Farrahshaida%20Mohd%20Salleh.pdf
id ukm-11395
recordtype eprints
spelling ukm-113952018-02-15T05:48:15Z http://journalarticle.ukm.my/11395/ Effect of space holders on fabrication of porous titanium alloy-hydroxyapatite composite through powder injection molding Farrahshaida Mohd Salleh, Abu Bakar Sulong, Muhammad Rafi Raza, Norhamidi Muhamad, Lim, Tsiu Fhang Powder injection molding (PIM) is able to produce porous titanium alloy/hydroxyapatite composite through the space holder technique. Thermal debinding and sintering processes were the main challenges due to different properties of metal and ceramic in producing such composite. This study focused on the effect of different space holders on the physical and mechanical properties of debound and sintered porous titanium aloi/hydroxyapatite composite. The feedstock is containing of 80 wt. % of titanium alloy/hydroxyapatite with 20 wt. % of space holders such as sodium chloride (NaCl) and polymethylmethacrylate (PMMA), respectively. The binders were then removed from the injected samples by two stages of debinding; solvent and thermal debinding. The sintering was performed at three different temperatures 1100oC, 1200oC and 1300oC at a heating rate of 10oC /min and holding time of 5 h. It was found that the samples containing PMMA space holder was fractured after sintering. While, the samples containing NaCl space holder successfully formed pores and not fractured. At sintering temperature of 1300oC, the density, compressive strength and porosity volume percentages for the sintered sample containing NaCl space holder were 3.05 g/cm3, 91.7 MPa. and 11.9 vol%, respectively. Penerbit Universiti Kebangsaan Malaysia 2017-09 Article PeerReviewed application/pdf en http://journalarticle.ukm.my/11395/1/38%20Farrahshaida%20Mohd%20Salleh.pdf Farrahshaida Mohd Salleh, and Abu Bakar Sulong, and Muhammad Rafi Raza, and Norhamidi Muhamad, and Lim, Tsiu Fhang (2017) Effect of space holders on fabrication of porous titanium alloy-hydroxyapatite composite through powder injection molding. Sains Malaysiana, 46 (9). pp. 1651-1657. ISSN 0126-6039 http://www.ukm.my/jsm/malay_journals/jilid46bil9_2017/KandunganJilid46Bil9_2017.html
repository_type Digital Repository
institution_category Local University
institution Universiti Kebangasaan Malaysia
building UKM Institutional Repository
collection Online Access
language English
description Powder injection molding (PIM) is able to produce porous titanium alloy/hydroxyapatite composite through the space holder technique. Thermal debinding and sintering processes were the main challenges due to different properties of metal and ceramic in producing such composite. This study focused on the effect of different space holders on the physical and mechanical properties of debound and sintered porous titanium aloi/hydroxyapatite composite. The feedstock is containing of 80 wt. % of titanium alloy/hydroxyapatite with 20 wt. % of space holders such as sodium chloride (NaCl) and polymethylmethacrylate (PMMA), respectively. The binders were then removed from the injected samples by two stages of debinding; solvent and thermal debinding. The sintering was performed at three different temperatures 1100oC, 1200oC and 1300oC at a heating rate of 10oC /min and holding time of 5 h. It was found that the samples containing PMMA space holder was fractured after sintering. While, the samples containing NaCl space holder successfully formed pores and not fractured. At sintering temperature of 1300oC, the density, compressive strength and porosity volume percentages for the sintered sample containing NaCl space holder were 3.05 g/cm3, 91.7 MPa. and 11.9 vol%, respectively.
format Article
author Farrahshaida Mohd Salleh,
Abu Bakar Sulong,
Muhammad Rafi Raza,
Norhamidi Muhamad,
Lim, Tsiu Fhang
spellingShingle Farrahshaida Mohd Salleh,
Abu Bakar Sulong,
Muhammad Rafi Raza,
Norhamidi Muhamad,
Lim, Tsiu Fhang
Effect of space holders on fabrication of porous titanium alloy-hydroxyapatite composite through powder injection molding
author_facet Farrahshaida Mohd Salleh,
Abu Bakar Sulong,
Muhammad Rafi Raza,
Norhamidi Muhamad,
Lim, Tsiu Fhang
author_sort Farrahshaida Mohd Salleh,
title Effect of space holders on fabrication of porous titanium alloy-hydroxyapatite composite through powder injection molding
title_short Effect of space holders on fabrication of porous titanium alloy-hydroxyapatite composite through powder injection molding
title_full Effect of space holders on fabrication of porous titanium alloy-hydroxyapatite composite through powder injection molding
title_fullStr Effect of space holders on fabrication of porous titanium alloy-hydroxyapatite composite through powder injection molding
title_full_unstemmed Effect of space holders on fabrication of porous titanium alloy-hydroxyapatite composite through powder injection molding
title_sort effect of space holders on fabrication of porous titanium alloy-hydroxyapatite composite through powder injection molding
publisher Penerbit Universiti Kebangsaan Malaysia
publishDate 2017
url http://journalarticle.ukm.my/11395/
http://journalarticle.ukm.my/11395/
http://journalarticle.ukm.my/11395/1/38%20Farrahshaida%20Mohd%20Salleh.pdf
first_indexed 2023-09-18T20:00:13Z
last_indexed 2023-09-18T20:00:13Z
_version_ 1777406797962805248