Scratch Adhesion and Wear Failure Characteristics of PVD multilayer CrTi/CrTiN Thin Film Ceramic Coating Deposited on AA7075-T6 Aerospace Alloy
This study highlights the scratch adhesion failure characterization and tribo-mechanical properties of physical vapor deposited (Cr, Ti) N coating on AA7075-T6 by using magnetron-sputtering technique. The surface morphology, microstructure and chemical composition of CrTi/CrTiN fim were inspected b...
Main Authors: | , , , , |
---|---|
Format: | Article |
Language: | English |
Published: |
Taylor & Francis
2018
|
Subjects: | |
Online Access: | http://umpir.ump.edu.my/id/eprint/19229/ http://umpir.ump.edu.my/id/eprint/19229/ http://umpir.ump.edu.my/id/eprint/19229/ http://umpir.ump.edu.my/id/eprint/19229/1/fkm-2018-mishak-Scratch%20Adhesion%20and%20Wear%20Failure%20Characteristics1.pdf |
id |
ump-19229 |
---|---|
recordtype |
eprints |
spelling |
ump-192292018-03-07T06:41:19Z http://umpir.ump.edu.my/id/eprint/19229/ Scratch Adhesion and Wear Failure Characteristics of PVD multilayer CrTi/CrTiN Thin Film Ceramic Coating Deposited on AA7075-T6 Aerospace Alloy Quazi, M. M. M., Ishak Arslan, A. M. Nasir, Bashir Imran, Ali TJ Mechanical engineering and machinery This study highlights the scratch adhesion failure characterization and tribo-mechanical properties of physical vapor deposited (Cr, Ti) N coating on AA7075-T6 by using magnetron-sputtering technique. The surface morphology, microstructure and chemical composition of CrTi/CrTiN fim were inspected by an optical microscope, scanning electron microscope (SEM) incorporated with energy dispersive X-ray spectroscopy (EDX) in addition to focused ion beam milling. The coating to substrate critical load of about 1261 mN was obtained, by employing coating deposition parameters of; DC power (300 W, RF power (200 W)), temperature (300 °C) and nitrogen flw rate (6%). Failure adhesion characteristics exhibited initial arc-tensile cracking followed by chipping and spallation that led to complete coating failure at Lc3. The tribo-mechanical aspects were evaluated by a pinon-plate reciprocating testing unit, which showed a lower friction coeffient of 0.36 for CrTiN as compared with 0.43 for AA7075-T6. Subsequently, the wear depth was also reduced from 9.5 to 5.9 μm. It was revealed that the wear mechanism for AA7075-T6 was extensive deformation, abrasion and delamination, while the CrTiN exhibited slightly oxidative abrasive wear mode. Taylor & Francis 2018-09-07 Article PeerReviewed application/pdf en http://umpir.ump.edu.my/id/eprint/19229/1/fkm-2018-mishak-Scratch%20Adhesion%20and%20Wear%20Failure%20Characteristics1.pdf Quazi, M. M. and M., Ishak and Arslan, A. and M. Nasir, Bashir and Imran, Ali (2018) Scratch Adhesion and Wear Failure Characteristics of PVD multilayer CrTi/CrTiN Thin Film Ceramic Coating Deposited on AA7075-T6 Aerospace Alloy. Journal of Adhesion Science and Technology, 32 (6). pp. 625-641. ISSN 0169-4243 https://doi.org/10.1080/01694243.2017.1373988 doi: 10.1080/01694243.2017.1373988 |
repository_type |
Digital Repository |
institution_category |
Local University |
institution |
Universiti Malaysia Pahang |
building |
UMP Institutional Repository |
collection |
Online Access |
language |
English |
topic |
TJ Mechanical engineering and machinery |
spellingShingle |
TJ Mechanical engineering and machinery Quazi, M. M. M., Ishak Arslan, A. M. Nasir, Bashir Imran, Ali Scratch Adhesion and Wear Failure Characteristics of PVD multilayer CrTi/CrTiN Thin Film Ceramic Coating Deposited on AA7075-T6 Aerospace Alloy |
description |
This study highlights the scratch adhesion failure characterization and tribo-mechanical properties of physical vapor deposited (Cr, Ti) N coating on AA7075-T6 by using magnetron-sputtering technique. The surface morphology, microstructure and chemical composition
of CrTi/CrTiN fim were inspected by an optical microscope, scanning electron microscope (SEM) incorporated with energy dispersive X-ray spectroscopy (EDX) in addition to focused ion beam milling. The coating to substrate critical load of about 1261 mN was obtained, by employing coating deposition parameters of; DC power (300 W, RF power (200 W)), temperature (300 °C) and nitrogen flw rate (6%). Failure adhesion characteristics exhibited initial arc-tensile cracking followed by chipping and spallation that led to complete coating failure at Lc3. The tribo-mechanical aspects were evaluated by a pinon-plate reciprocating testing unit, which showed a lower friction coeffient of 0.36 for CrTiN as compared with 0.43 for AA7075-T6. Subsequently, the wear depth was also reduced from 9.5 to 5.9 μm. It was revealed that the wear mechanism for AA7075-T6 was extensive deformation, abrasion and delamination, while the CrTiN exhibited slightly oxidative abrasive wear mode. |
format |
Article |
author |
Quazi, M. M. M., Ishak Arslan, A. M. Nasir, Bashir Imran, Ali |
author_facet |
Quazi, M. M. M., Ishak Arslan, A. M. Nasir, Bashir Imran, Ali |
author_sort |
Quazi, M. M. |
title |
Scratch Adhesion and Wear Failure Characteristics of PVD multilayer CrTi/CrTiN Thin Film Ceramic Coating Deposited on AA7075-T6 Aerospace Alloy |
title_short |
Scratch Adhesion and Wear Failure Characteristics of PVD multilayer CrTi/CrTiN Thin Film Ceramic Coating Deposited on AA7075-T6 Aerospace Alloy |
title_full |
Scratch Adhesion and Wear Failure Characteristics of PVD multilayer CrTi/CrTiN Thin Film Ceramic Coating Deposited on AA7075-T6 Aerospace Alloy |
title_fullStr |
Scratch Adhesion and Wear Failure Characteristics of PVD multilayer CrTi/CrTiN Thin Film Ceramic Coating Deposited on AA7075-T6 Aerospace Alloy |
title_full_unstemmed |
Scratch Adhesion and Wear Failure Characteristics of PVD multilayer CrTi/CrTiN Thin Film Ceramic Coating Deposited on AA7075-T6 Aerospace Alloy |
title_sort |
scratch adhesion and wear failure characteristics of pvd multilayer crti/crtin thin film ceramic coating deposited on aa7075-t6 aerospace alloy |
publisher |
Taylor & Francis |
publishDate |
2018 |
url |
http://umpir.ump.edu.my/id/eprint/19229/ http://umpir.ump.edu.my/id/eprint/19229/ http://umpir.ump.edu.my/id/eprint/19229/ http://umpir.ump.edu.my/id/eprint/19229/1/fkm-2018-mishak-Scratch%20Adhesion%20and%20Wear%20Failure%20Characteristics1.pdf |
first_indexed |
2023-09-18T22:27:34Z |
last_indexed |
2023-09-18T22:27:34Z |
_version_ |
1777416068577361920 |